Carbide saw blade grinding surface and in accordance with rake angle of the surface after a 1:3 relationship, only when the saw blade through the right to make the tool after grinding to maintain normal working life. Incorrect grinding, if only the front face or only from granite polishing pads a corner after corner knife surface grinding tool life will be shortened. Another important point is that the whole area should be fully worn grinding. Carbide saw blade sharpening machine is placed on automatic grinding, due to quality reasons, we do not recommend universal grinding machine grinding blade manually, automatic CNC grinding performance guarantee rake surface and the surface of the posterior horn of the repair mill entirely in the tamping rammer same direction.
Rake surface and the posterior horn of the surface grinding carbide teeth ensure ideal working condition and stable life, serrated remaining length and width should be at least not less than 1 mm (measured starting from tooth Block).
Saws grinding
To prevent large diamond dressing grinding wheel wear, it is necessary to saw the side of the sawtooth sufficient living a side projecting portion. On the other hand, the maximum lateral projection on each side should not exceed 1.0 to 1.2 mm in order to ensure the stability of the ceramic tile saw sawtooth.
Changes flute
Despite grinding reduces jagged length, but YFENG flute design ensures heat off of the saw blade grinding operation has sufficient chip space, thus avoiding grinding teeth grinding while the flutes to the case .
Diamond tool is mainly used for a variety of non-ferrous metals such as aluminum turning, copper, magnesium and its alloys, tungsten carbide and wear strong fiber reinforced plastic materials, metal matrix composites, wood and other non-metallic materials. When cutting speed, feed rate and depth of cut depends on processing conditions and the hardness of the workpiece material.